A217 WC9

ASTM:
A217 WC9
ASME:
SA217 WC9
Alloy Family:
Type:
Designation:
ACI:
AISI:
SAE:
UNS - Cast:
J21890
UNS - Wrought:
Common Name - Wrought:

Alloy Casting Statistics

Pounds Poured in 2021

6,600 lb

Frequently Asked Questions

No frequently asked questions available for this alloy. Have one? Email us at faq@alloycasting.com to get your answers.
Alloy Casting Industries Ltd makes all reasonable efforts to ensure the accuracy and correctness of the data displayed on this site but makes no representations or warranties as to the data’s accuracy, correctness or reliability. The information provided on this page is for reference purposes only. Please consult the appropriate industry standard when necessary.

Industry Standard

Chemical Composition

  • Carbon:
    0.05 - 0.18%
  • Manganese:
    0.40 - 0.70%
  • Silicon:
    0.60% Max
  • Phosphorus:
    0.035% Max
  • Sulfur:
    0.035% Max
  • Chromium:
    2.00 - 2.75%
  • Nickel:
    0.50% Max
  • Molybdenum:
    0.90 - 1.20%
  • Nitrogen:
  • Nitrogen + Carbon:
  • Vanadium:
  • Tungsten:
    0.10% Max
  • Aluminum:
  • Titanium:
  • Copper:
    0.50% Max
  • Columbium:
  • Barium:
  • Boron:
  • Zirconium:
  • Cerium + Lanthanum:
  • Iron:
  • Residual Elements:
    1.00% Max

Physical Properties

  • Yield Strength:
    40 ksi Min
  • Tensile Strength:
    70 - 95 ksi
  • Elongation at 2 in:
    20% Min
  • Reduction of Area:
    35% Min

Charpy Properties

  • Test Temperature:
  • Average Energy¹:
  • Single Energy: